Which materials does MWA machine?
MWA machines structural steel, quenched and tempered steel and case-hardening steel, grey cast iron, ductile (nodular) cast iron, cast steel, stainless steel, aluminum, bronze, brass and titanium. Typical grades are S355J2 (1.0577), 42CrMo4 (1.7225), 16MnCr5 (1.7131), EN-GJS-400-15 (EN-JS1030), 1.4404, duplex 1.4462, EN AW-6082 and Ti6Al4V (3.7165). For other materials, please ask us directly; we check machinability on a case-by-case basis. If possible, specify the material with its material number or standard designation.
Do you procure the material or do I have to supply it?
Both are possible: we procure the material ourselves or machine material supplied by you. If we procure it, the material is included in the quote, with a material certificate according to EN 10204 on request. Supplying material yourself makes sense if you want to use special materials, blanks such as castings or forgings, or existing stock. Please state in your inquiry which option you prefer.
What is the difference between 1.4301 and 1.4404?
1.4404 additionally contains molybdenum and is therefore more resistant to chloride-containing media than 1.4301. 1.4301 (X5CrNi18-10, AISI 304, colloquially known in German as V2A) is the most widely used austenitic stainless steel for general applications. 1.4404 (X2CrNiMo17-12-2, AISI 316L, often called V4A) is used with salt water, chemicals or in food processing technology. Both are tough and tend to work-harden during machining.
Which stainless steel is easiest to machine?
Among the austenitic stainless steels, 1.4305 (X8CrNiS18-9, AISI 303) is considered particularly easy to machine. The added sulfur produces short chips but reduces corrosion resistance and weldability. For parts that will be welded or operate in an aggressive environment, 1.4301 or 1.4404 is usually the better choice. Which material is suitable therefore depends on the application, not only on machinability.
What is the difference between 1.4571 and 1.4404?
1.4571 (X6CrNiMoTi17-12-2) is stabilized with titanium, whereas 1.4404 (X2CrNiMo17-12-2) achieves its resistance to intergranular corrosion through a low carbon content. Both contain molybdenum and have similar resistance in chloride-containing environments. 1.4571 is traditionally widespread in Germany in apparatus and plant engineering, while 1.4404 is used more frequently internationally and is easier to polish. The titanium carbides in 1.4571 noticeably increase tool wear during machining.
What is duplex steel 1.4462?
1.4462 (X2CrNiMoN22-5-3) is a duplex stainless steel with a microstructure of roughly equal proportions of austenite and ferrite. It has significantly higher strength than 1.4404 and is particularly resistant to pitting and stress corrosion cracking, for example in seawater, offshore installations and chemical engineering. It is more demanding to machine than standard austenitic grades and requires rigid setups and adapted cutting parameters. MWA machines 1.4462 to drawing.
What does EN AW-6082 mean and which aluminum alloy is suitable for milled parts?
EN AW-6082 (AlSi1MgMn, formerly 3.2315) is a heat-treatable aluminum alloy with good strength, good machinability and good weldability. It is a solid standard choice for many milled parts in mechanical engineering, usually in temper T6 or T651. EN AW-7075 (AlZn5,5MgCu) is considerably stronger but hardly weldable. EN AW-5083 (AlMg4,5Mn0,7) is not heat-treatable and is particularly resistant to seawater. EN AW stands for wrought aluminum alloy according to the European standard.
What is Ti6Al4V and do you machine titanium?
Ti6Al4V is the most widely used titanium alloy, also known as Grade 5 or by material number 3.7165. It contains about 6 percent aluminum and 4 percent vanadium and combines high strength with low density and good corrosion resistance. Because of its low thermal conductivity, titanium is considered demanding to machine. MWA machines titanium; send us your drawing and requirements for a feasibility check.
What is the difference between S235 and S355?
The number indicates the minimum yield strength in N/mm²: S235 has 235 N/mm² and S355 has 355 N/mm² for product thicknesses up to 16 mm. S355 can therefore bear considerably higher loads and is preferred for load-bearing parts and machine frames. The code letters describe the impact energy: JR means 27 joules at +20 °C, J2 means 27 joules at −20 °C. Common grades are S235JR (1.0038) and S355J2 (1.0577), both readily weldable and machinable.
What is a quenched and tempered steel such as C45, 42CrMo4 or 34CrNiMo6?
Quenched and tempered steels are steels that obtain high strength combined with good toughness through hardening followed by tempering. C45 (1.0503) is unalloyed and is frequently used for shafts and pins. 42CrMo4 (1.7225) is alloyed and can be through-hardened and tempered even in larger cross-sections. 34CrNiMo6 (1.6582) additionally contains nickel and is suitable for highly stressed parts with large cross-sections. Steels supplied in the quenched and tempered condition are designated +QT.
What is a case-hardening steel such as 16MnCr5 or 18CrNiMo7-6?
Case-hardening steels are low-carbon steels whose surface layer becomes wear-resistant through carburizing and hardening, while the core remains tough. 16MnCr5 (1.7131) is a widely used standard grade for gears, pins and medium-sized shafts. 18CrNiMo7-6 (1.6587) is more highly alloyed, hardens to a greater depth and is used for highly loaded gearbox parts with larger cross-sections. Machining is usually done before case hardening; functional surfaces are often ground afterwards.
Do you machine brass and which brass is common?
Yes, MWA machines brass to drawing. For turned parts, CW614N (CuZn39Pb3) is widespread, a free-cutting brass that is very easy to machine thanks to its lead content. For applications with requirements on lead content, for example in drinking water systems, low-lead brass grades are available. Please state the exact material designation so that we can procure the right semi-finished product.
Which bronzes are common for plain bearings and bushings?
Tin bronzes and aluminum bronzes are common for plain bearings and bushings. CuSn12-C (CC483K) is a cast tin bronze for highly loaded plain bearings and worm wheels, and CuSn8 (CW453K) is a wrought alloy for bushings and sliding elements. CuAl10Ni5Fe4 (CW307G) is a multi-component aluminum bronze with high strength and good resistance to seawater and wear. MWA machines bronze as bar stock and as cast blanks; please state the exact material designation.
What do EN-GJL and EN-GJS mean for cast materials?
EN-GJL designates cast iron with lamellar graphite (grey cast iron), and EN-GJS designates cast iron with spheroidal graphite (ductile (nodular) cast iron). The number that follows is the minimum tensile strength in N/mm²; for GJS, it is followed by the elongation at break in percent. Common grades are EN-GJL-250 (EN-JL1040) and EN-GJS-400-15 (EN-JS1030). Grey cast iron dampens vibrations well and is typical for housings and machine beds, while ductile cast iron is tougher and can bear higher loads. MWA machines both cast materials, including as customer-supplied blanks.
What is cast steel and how is it designated?
Cast steel is steel cast in molds, combining the strength and weldability of steel with the design freedom of a casting. The short designations according to EN 10293 begin with G, for example GE240 (1.0446) as an unalloyed cast steel for general applications or G20Mn5 (1.6220) with good toughness and weldability. Cast steel is tougher than cast iron but dampens vibrations less than grey cast iron. Typical components are housings, bearing blocks, hubs and levers.
Materials, tubes and processes in detail
Which steel tubes are there and what are they used for?
The main types are seamless, welded and precision steel tubes. Seamless tubes to EN 10216 or EN 10297-1 suit high pressures and heavily loaded parts such as bushings and shafts, while welded tubes to EN 10217 or EN 10219 are economical for structures and frames. Precision steel tubes to EN 10305 have tight dimensional tolerances, for example for hydraulics and cylinders. We work out with you which tube type suits your part and confirm availability and dimensions for each enquiry.
What are precision steel tubes to EN 10305?
Precision steel tubes are cold-drawn tubes with tight dimensional tolerances and a smooth surface. EN 10305-1 covers seamless and EN 10305-2 welded and drawn precision tubes. Typical applications are hydraulics, cylinders and guides. On request, we supply them cut to size or machine them directly.
Do you supply square and rectangular tubes (hollow sections)?
Yes, hollow sections are one of the forms of supply in our commodity trading. Square and rectangular tubes are supplied to EN 10210 (hot finished) or EN 10219 (cold formed), usually in S235JRH or S355J2H. We confirm dimensions and availability for each enquiry, cut to size on request.
What is the difference between material number and steel name?
The steel name, for example 42CrMo4, describes the composition or properties of a steel; the material number to EN 10027-2, for example 1.7225, is a unique sequence of digits for the same material. The first digit 1 stands for steel and the next two for the steel group; 1.40 to 1.45, for example, are stainless steels. One of the two is enough in your enquiry.
What are the tool steels 1.2379 and 1.2312?
1.2379 (X153CrMoV12) is a wear-resistant cold work steel for cutting and punching tools, knives and wear parts. 1.2312 (40CrMnMoS8-6) is a pre-hardened, easily machinable steel for moulds, mould frames, fixtures and machine parts. We supply both through our commodity trading and machine them in our contract manufacturing.
What is the difference between EN AW-6082 and EN AW-7075?
EN AW-6082 is an easily weldable aluminium alloy with good strength and corrosion resistance, while EN AW-7075 is one of the strongest aluminium alloys but has only limited weldability. 6082 is used for structural parts and fixtures, 7075 in aerospace, mould making and highly stressed lightweight parts. Both are available, for example, as plates for milled parts.
Which inspection documents are there according to EN 10204?
EN 10204 defines the documents 2.1, 2.2, 3.1 and 3.2. 2.1 only declares compliance with the order, 2.2 contains typical values from ongoing production, 3.1 results of specific inspection on the delivered batch, and with 3.2 a representative of the purchaser or a notified body also confirms the results. At MWA you receive 2.2 or 3.1 on request; for safety-relevant parts we recommend 3.1.
What is the difference between simultaneous and indexed 5-axis machining?
In simultaneous 5-axis machining all five axes move at the same time, for example for freeform surfaces; in indexed (3+2) machining the workpiece is tilted into a fixed angle and then machined on three axes. Both save re-clamping and increase accuracy. MWA uses both, depending on which is more economical for your part.
What is thread milling?
In thread milling a rotating milling tool produces the thread with a circular movement instead of cutting it with a tap. This is reliable and also suits large thread diameters. We use thread milling when clean, reliable threads are the priority.
What do boring and fine boring of bearing seats mean?
Boring and fine boring are processes that bring large bores such as bearing seats to exact size with a good surface. They are mainly used for housings, gearboxes and machine beds. At MWA they run on boring mills, often together with jig boring of precise hole patterns in just a few set-ups.
What are cylindrical and profile grinding?
Cylindrical grinding machines cylindrical surfaces particularly accurately and smoothly, outside on shafts or inside in bores (internal grinding). Profile grinding produces special contours. Both are used when functional surfaces such as bearing seats, sealing surfaces or guideways place high demands on size and surface.
Do you also handle storage, logistics and customs clearance?
Yes, in commodity trading we deliver on request including storage, logistics and customs clearance. This way you receive material on time and with a material certificate without having to keep storage space yourself. Tell us your requirements and we will agree the handling with you.
Material, cutting to size and machining
In which forms can I get the material?
Depending on the material and intended use, we supply round bar, flat bar and square bar, sheets and plates, for example aluminium plates in EN AW-6082 or EN AW-7075, as well as tubes, hollow sections and cut-to-size pieces to your dimensions. Raw castings and forgings are sourced through our partner network. On request, you receive the finished machined component directly from our contract manufacturing. Other materials, dimensions and forms are available on request.
What information do you need for cutting to size?
For a quote we need the material (designation or material number) and, if applicable, the standard, the dimensions or cross-section and the length per piece, the quantity and required tolerance, the inspection certificate you need (EN 10204 2.2 or 3.1), and the delivery date and location. Cutting to size saves you offcuts, storage space and your own working time.
What is the difference between titanium Grade 2 and Grade 5?
Grade 2 is commercially pure titanium with very good corrosion resistance, used for example in chemical and plant engineering. Grade 5 (Ti6Al4V) is the most widely used titanium alloy, with high strength for aerospace, medical technology and special applications. Both are light (around 4.5 g/cm³), highly corrosion-resistant and biocompatible.
How does a material inquiry in commodity trading work?
You tell us the material, dimensions, form, quantity, certificate and date, ideally with a drawing. We check availability and alternatives and clarify any open points. You then receive a quote for material, cutting and, on request, machining. Delivery is on schedule with an inspection certificate and, on request, including storage, logistics and customs clearance. More on the commodity trading page.
Which components are suited to CNC milling?
Milling is suited to prismatic components with flat faces, pockets, slots, contours and hole patterns, for example plates, housings, brackets, bearing blocks and fixtures. This includes face, contour, slot and pocket milling, thread milling and 3D form milling from a 3D model, for long and heavy workpieces also on the boring mill.
Which components are suited to CNC turning?
Turning is the process for rotationally symmetrical components such as shafts, axles, pins, bushings, flanges and rings. We use short and long turning for shafts and axles, facing and internal turning for flanges, bushings and bores, and thread turning for external and internal threads.
Do you also repair worn shafts and components?
Yes, shaft repair and the reconditioning of worn components are part of our turning services. Ideally, send us photos, any existing drawings and a short description of the damage via the contact form; we will then check how the component can be repaired.
What is jig boring (coordinate drilling)?
Jig boring produces holes at precisely defined distances from each other, in other words accurate hole patterns. Together with boring out and fine boring of bearing seats as well as tapping, reaming and countersinking, it is part of our drilling and horizontal boring work, for example for large housings, gearboxes and machine beds.
Why should I state the annual quantity for recurring demand?
Programming and set-up are incurred once per order. If we know your expected annual quantity, we can plan batch sizes economically so that these costs are spread over more parts. So feel free to state the annual quantity in your inquiry.
Choosing the right material in practice
Which steel is suitable for heavily loaded shafts with a large diameter?
For heavily loaded shafts and components with large diameters, the quenched and tempered steels 42CrMo4 (1.7225) and 34CrNiMo6 (1.6582) are suitable. 34CrNiMo6 additionally contains nickel and remains very tough even in large cross-sections. The larger the cross-section and the higher the load, the more likely one of these two materials is chosen instead of C45.
Which material is suitable for gears and gearbox parts?
For gears, camshafts and shafts with gearing, the case-hardening steel 16MnCr5 (1.7131) is the standard. For heavily loaded gearbox parts with larger dimensions, for example in wind turbine and industrial gearboxes, the higher-alloyed 18CrNiMo7-6 (1.6587) is used. Both are case-hardened after machining, creating a hard, wear-resistant surface layer with a tough core.
Which stainless steel is resistant to salt water and cleaning agents?
The molybdenum-containing stainless steels 1.4404 and 1.4571 are more resistant to chloride-containing media such as salt water or cleaning agents than 1.4301. Where high strength is also required, for example offshore, in the chemical industry or in marine engineering, duplex 1.4462 is suitable, with very good resistance to pitting and stress corrosion cracking.
Which cast material is suitable for machine beds and housings?
Grey cast iron EN-GJL-250 damps vibrations very well and is therefore ideal for machine beds, housings and base plates. Where higher strength and toughness are required, for example for hubs, bearing housings and gearbox parts, ductile iron such as EN-GJS-400-15 or EN-GJS-600-3 is used. We source raw castings through our partner network and, on request, finish-machine them in our contract manufacturing.
When is aluminium a better choice than steel?
Aluminium weighs about one third as much as steel and can be machined economically at high cutting speeds. EN AW-6082 offers good strength, corrosion resistance and weldability for structural parts and fixtures. EN AW-7075 is one of the strongest aluminium alloys and is suitable for highly loaded lightweight components, but it has only limited weldability.
In which delivery condition do I receive quenched and tempered steel?
Quenched and tempered steels such as C45, 42CrMo4 or 34CrNiMo6 gain high strength with good toughness through hardening and tempering. We agree the suitable delivery condition with you when you send your enquiry, for example quenched and tempered or soft annealed. You can find more about the materials on our commodity trading page.
Which material is suitable for cutting tools or moulds?
For cutting and punching tools, knives and wear parts, the wear-resistant cold work tool steel 1.2379 (X153CrMoV12) is suitable. For moulds, mould frames, fixtures and machine parts, the pre-hardened, easily machinable steel 1.2312 (40CrMnMoS8-6) is frequently used.
Which stainless steel tubes do you supply?
We supply stainless steel tubes made of 1.4301, 1.4404 or 1.4571, seamless according to EN 10216-5 or welded according to EN 10217-7. They are used wherever corrosion resistance is required. We state availability and dimensions for each enquiry, including cutting to size and machining on request.
What do you pay attention to when machining austenitic stainless steel?
Austenitic stainless steels such as 1.4301 or 1.4404 tend to work-harden during machining. We take this into account when choosing tools and cutting parameters so that dimensions and surface finish are right. Feel free to send us your drawing via our contact page.
Hardening, heat treatment and surface finishes briefly explained
What is the difference between hardening and quenching and tempering?
In hardening, steel is heated to a high temperature and then cooled rapidly. This makes the microstructure very hard, but also brittle. In quenching and tempering, hardening is followed by tempering at a higher temperature. The part loses some hardness, but in return becomes considerably tougher and more resilient. Quenching and tempering is used above all for shafts, pins and axles made of quench and temper steel; hardening is used above all for parts that need to be wear-resistant. The drawing should state which process is meant and which hardness or strength is required.
What does tempering after hardening mean?
Tempering means reheating the part after hardening, well below the hardening temperature. It relieves stresses in the microstructure and makes the hardened steel less brittle. The higher the tempering temperature, the softer and tougher the part becomes. Without tempering, hardened parts can crack under load or even during grinding. That is why hardening and tempering practically always go together.
What is case hardening?
In case hardening, the surface layer of a low-carbon steel is enriched with carbon and then hardened. This creates a hard, wear-resistant surface over a tough core. It is typical for gears, pins and shafts that are subject to high stress at the surface. The drawing specifies the surface hardness and the case hardening depth, abbreviated CHD. Suitable materials are case-hardening steels such as 16MnCr5, which are described in the Materials category.
What is induction hardening?
In induction hardening, only a specific area of a part is rapidly heated by an electromagnetic field and immediately quenched. This allows a bearing seat, a raceway or a gear toothing to be hardened selectively, while the rest of the part remains unchanged. The process is suitable for quench and temper steels such as C45 or 42CrMo4. The drawing states the required hardness, the hardening depth and the exact area to be hardened.
What is nitriding?
In nitriding, nitrogen is introduced into the surface of the steel. This creates a thin, very hard and wear-resistant layer. Because the temperature is lower than in hardening, the parts hardly distort. Nitriding is therefore suitable for finish-machined parts with tight tolerances, such as spindles, guides or mould components. There are gas nitriding, plasma nitriding and nitrocarburising. Which process is suitable depends on the material and the application.
In what order are machining and hardening planned?
Usually a part is first turned or milled in the soft state, leaving a machining allowance at important points. This is followed by the heat treatment. Because the part may distort slightly in the process, fits and bearing seats are only ground or hard-turned to final dimension afterwards. With quench and temper steel that is already supplied in the quenched and tempered condition, this step is often not needed. MWA plans the sequence so that enough material remains for finish machining after the heat treatment. More on this under Turning and grinding.
What is the difference between zinc electroplating and hot-dip galvanising?
In zinc electroplating, a thin layer of zinc is applied electrochemically. The coating is uniform and suitable for smaller precision parts, screws and threads. In hot-dip galvanising, the part is dipped into molten zinc. The coating is much thicker and protects for longer, for example in steel construction or outdoors. Because of the coating thickness, hot-dip galvanising is usually unsuitable for fits and threads. The drawing should state which process and which coating thickness are required.
Why does anodising change the dimensions of an aluminium part?
In anodising, the surface of aluminium is converted electrochemically into a hard oxide layer. Roughly half of the layer grows into the material and half grows outwards. External dimensions therefore become slightly larger, holes slightly smaller. With standard anodising this is usually negligible, but not with hard anodising, which has a thicker layer. For tight fits, the drawing should therefore specify whether a dimension applies before or after anodising. Alloys such as EN AW-6082 are well suited.
Material designations, semi-finished products and testing briefly explained
What is free-cutting steel such as 11SMn30 and what is it suitable for?
Free-cutting steels are steels with an increased sulphur content, some with added lead, for example 11SMn30 (1.0715) or 11SMnPb30 (1.0718). In turning, the sulphur produces short chips and allows high cutting speeds. That is why these steels are widely used for turned parts in larger quantities, such as pins, bushes and threaded fittings. The downside: free-cutting steel is difficult to weld and is less tough than a structural steel or a quenched and tempered steel. For highly stressed, welded or pressure-bearing parts it is therefore usually not the right choice. With leaded grades, you should also check whether your product is subject to substance restrictions such as RoHS.
What is the difference between bright steel and hot-rolled steel?
Hot-rolled steel comes from the rolling mill with a dark layer of mill scale and comparatively coarse dimensional tolerances. Bright steel is subsequently cold drawn, peeled or ground. It has a smooth, bright metallic surface and tight dimensional tolerances, for round bar for example h9 or h11. The technical delivery conditions are given in EN 10277, the dimensions and tolerances in EN 10278. Bright steel often saves machining because the outside diameter can be used as it is. Drawn material does, however, contain residual stresses: if a lot of material is removed on one side, for example for a long keyway, the part can distort. Hot-rolled material is cheaper and common in large sizes, but needs more machining allowance.
What does the designation S355J2+N mean for structural steel?
The designation follows the standard EN 10025-2. S stands for structural steel, 355 for the minimum yield strength of 355 MPa at small product thicknesses. J2 describes the toughness: in the Charpy impact test the steel must absorb at least 27 joules at −20 °C. JR means 27 joules at +20 °C, J0 at 0 °C and K2 at least 40 joules at −20 °C. The suffix +N indicates the delivery condition: normalised or normalising rolled. +AR, by contrast, means “as rolled”. For components that are welded and exposed to lower temperatures, S355J2+N is frequently specified. State the full designation in your enquiry, because the material and the certificate are derived from it.
What are cast aluminium plates and when are they used instead of rolled plates?
Cast aluminium plates, often called precision plates, are cast and then face-milled on both sides. They are very low in residual stress, have a tight thickness and flatness tolerance and hardly distort during machining. That is why they are a popular choice for fixtures, base plates, machine tables and parts with large pockets. Rolled plates, for example in EN AW-5083, EN AW-6082 or EN AW-7075, have a higher strength. However, they carry residual stresses from rolling and can distort when a large volume of material is removed. Cast plates are less strong and are suitable for decorative anodising only to a limited extent. The deciding factor is therefore whether dimensional stability or strength is the priority.
What do tensile strength Rm, yield strength Re and proof strength Rp0.2 mean?
All three values come from the tensile test to ISO 6892-1 and are given in MPa (equivalent to N/mm²). The tensile strength Rm is the highest stress the test piece withstands before it necks and breaks. The yield strength Re marks the point from which the material deforms permanently. Many materials, such as aluminium, austenitic stainless steel or quenched and tempered steels, do not show a pronounced yield point. For these, the proof strength Rp0.2 is given: the stress at which 0.2% permanent elongation remains. The elongation after fracture A, in percent, additionally shows how ductile the material is. For design purposes, Re or Rp0.2 is usually what counts. The measured values of a heat are stated in the inspection certificate 3.1.
What does “ultrasonically tested” mean for steel bar and forgings?
Ultrasonic testing is a non-destructive method that finds internal defects such as shrinkage cavities, cracks or larger inclusions without damaging the material. A probe sends sound waves into the workpiece. Defects reflect part of the sound and thus become visible. EN 10308 applies to steel bar, EN 10228-3 to steel forgings and EN 10160 to plate. The standards define quality classes that specify which indications are still permissible. The test is particularly worthwhile for highly stressed shafts, large diameters and safety-relevant components. The requirement must already be fixed when the material is ordered and is confirmed in the certificate. You should therefore state the standard and quality class in your enquiry.
What do heat traceability and transfer of marking mean?
Every melt in the steel or aluminium works is given a heat number, also called a cast number. It appears in the inspection certificate 3.1 and as a stamp, print or label on the material. Traceability means that a component can be traced back via this number to the certificate and to the melt. When a bar or plate is cut to size, some of the cut pieces lose the original marking. In the transfer of marking, also known as re-stamping, the marking is therefore transferred to each piece before cutting. For certain applications, such as pressure equipment, this may only be done by a person authorised to do so, who certifies the operation. State in your enquiry if traceability down to the individual part is required, for example by marking each component.
Why can stainless steel still rust?
Stainless steel resists rust because, from about 10.5% chromium, a very thin, invisible passive layer of chromium oxide forms. If this layer is disturbed, stainless steel can rust too. The most common cause is extraneous rust: iron particles from tools, grinding dust or steel chips settle on the surface and rust there. Chlorides from salt water, de-icing salt or some cleaning agents can trigger localised pitting corrosion. Heat tint next to weld seams and narrow crevices are also susceptible. The remedy is clean tools kept separate from steel, thorough cleaning, and pickling and passivation. In a chloride-containing environment, a molybdenum-bearing steel such as 1.4404 performs better than 1.4301.
More FAQ topics
Your question is not listed?